- Details
- Factory Video
- Competitive Advantage
- Packing & Shipping
1)38CrMoAlA(JIS SACM645)
2)9Cr18MoV
1) 38CrMoAlA(JIS SACM645)
2) 9Cr18Mo
Heat-treatment
Nitriding treatment
Spray bimetallic coating
Quideline of technique
Depth of nitration layer: 0.05~0.08mm
Hardness of nitration: 900~1000hv
Fragility of nitration: less than grand one
Roughness of the surface: Ra0.4
Linearity of the screw: 0.015mm/m
The surface hardness of chrom plating after nitrogention:more than 950hv
Chrome-plating layer thickness:0.025~0.085mm